Being frosted, the Mylar already has a tooth. I only use it for sketches and very small works. I have never seen a need to prime it. I paint on canvas when I work larger.
__________________
www.WilliamWhitaker.com
  Reply With Quote
Old 03-20-2009, 09:35 AM   #2
Evan Shipard Evan Shipard is offline
Juried Member
 
Joined: Mar 2009
Location: Sydney, Australia
Posts: 5
Thanks Bill, btw Alex's work can be found here...
http://www.somepaintings.net/Alex.html
__________________
evan

___________________________
http://www.evanshipardfineart.com/
  Reply With Quote
Old 03-20-2009, 10:40 AM   #3
William Whitaker William Whitaker is offline
BOARD ADVISOR
SOG Member
FT Professional
 
William Whitaker's Avatar
 
Joined: Sep 2001
Location: Provo, UT
Posts: 397
Thank you for the link Evan. Alex Kanevsky is a terrific and inspiring painter and I've been following his work for some time, It was very thoughtful of you to provide the link.
__________________
www.WilliamWhitaker.com
  Reply With Quote
Old 03-20-2009, 09:59 PM   #4
Evan Shipard Evan Shipard is offline
Juried Member
 
Joined: Mar 2009
Location: Sydney, Australia
Posts: 5
Alex Kanevsky is an inspiration.

Ive just contacted Dupont but am having a hard time tracking mylar film down in Sydney. What thicknesses does it come in?
__________________
evan

___________________________
http://www.evanshipardfineart.com/
  Reply With Quote
Old 03-21-2009, 01:29 AM   #5
William Whitaker William Whitaker is offline
BOARD ADVISOR
SOG Member
FT Professional
 
William Whitaker's Avatar
 
Joined: Sep 2001
Location: Provo, UT
Posts: 397
I don't know. I don't have specifications here. I know it comes in various thicknesses. Sometimes it's frosted on one side only, sometimes on both sides. In thickness, mine compares with a nice sheet of drawing paper.
__________________
www.WilliamWhitaker.com
  Reply With Quote
Old 03-21-2009, 11:04 AM   #6
David Clemons David Clemons is offline
Juried Member
 
Joined: Feb 2007
Location: Austin, TX
Posts: 50
There are several other manufacturers of drafting film, such as Grafix, Azon, or Alvin. They're all pretty much identical. 3 mil thickness is common, up to 5 mil I think, but once mounted it doesn't much matter. I've used an acrylic gel as an adhsive and it works fine. The single sided matte is slightly cheaper than double sided. There's another film type made of polypropylene (Borden & Riley's Denril brand) that is almost identical. Also, drafting "vellum" is made of cotton fiber rather than synthetic. Canson makes a Opalux brand of this, and there are others. It's not as tear resistant as Mylar, but otherwise about the same.
__________________
David Clemons

http://www.dbclemons.com/
  Reply With Quote
Reply


Currently Active Users Viewing this Topic: 1 (0 members and 1 guests)
 

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off

Forum Jump

Similar Topics
Thread Topic Starter Forum Replies Last Post
CSOPA - Marvelous Mattelson demo Jeanine Jackson Upcoming Events & Announcements 2 02-23-2003 01:06 PM

 

Make a Donation



Support the Forum by making a donation or ordering on Amazon through our search or book links..







All times are GMT -4. The time now is 02:12 AM.


Powered by vBulletin® Version 3.8.6
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.